Reasons for the Poor Durability of H13 Shear Blades
May 09, 2026

Reasons for the Poor Durability of H13 Shear Blades

In common heat treatment standards, technical requirements often specify only the hardness range. To reduce costs, outsourced heat treatment providers frequently focus solely on meeting this hardness requirement. During the heat treatment process, if the heating temperature or soaking time is insufficient, the alloying elements in the tool steel cannot fully dissolve into the austenite. This results in an inadequate quenched and tempered microstructure, leading to defects such as edge deformation (collapsing) and loss of shape during service.


Solutions:
1.Conditioning Treatment: Subject the blade blanks to a preliminary quenching and tempering (conditioning) process to obtain an ideal pearlitic structure.

2.Graded Preheating: Implement multi-stage preheating and optimized soaking times to ensure the alloying elements are fully austenitized.
Newsletter

Veuillez lire ce qui suit, vous tenir informé, abonnez-vous, et nous vous souhaitons la bienvenue pour nous dire ce que vous en pensez.

Laisser un message
bienvenue Licheng
Si vous êtes intéressé par nos produits et souhaitez connaître plus de détails,veuillez laisser un message ici,nous vous répondrons dès que nous le pouvons.

Accueil

Produits

sur

contact